Tinning before Lead Free Solder

Viewing 1 post (of 1 total)
  • Author
    Posts
  • #30002
    mattschwier
    Member

    After applying the tinning butter to clean panel, I heat it w/ oxy/acet torch. I am left with shiny stuff (good) and brown crap (bad). What is the proper way to clean off the brown gunk?

Viewing 1 post (of 1 total)
  • You must be logged in to reply to this topic.