This was a chrome battery box cover. We coated, laid it flat in the oven, got it up to 450 degress, cured at 400 degrees for 20 minutes. It was perfect, then we noticed some areas that hadn’t gotten enough power so decided to shoot it again. Let cool, then the same process as the first time, came out Way messed up. Wrinkles and spread out places and zits.
This is one of the very first things I ever powder coated, and would like to know where I messed up
Thanks