rough finish

Posted: July 7, 2006 By: steviek

Home Forums Ask Eastwood Ask Eastwood Archives rough finish

Viewing 1 post (of 1 total)
  • Author

    Posts

  • #29668

    steviek

    Member

    can anyone help , when i put part into ovan at flowout temp 400 it goes rough instead of nice and smooth , i dont think i have been doing any thing differant than before when it flowed out fine .