Pitted Surface Repair

Viewing 1 post (of 1 total)
  • Author
    Posts
  • #32610
    GregAW
    Member

    I need some help. I’ve got some nickle plated aluminum that I was to powder coat. The problem it’s been sitting out in the weather and the nickle has pitted down to the aluminum. I’ll sandblast first but I think the pitting is going to be too deep to get a really nice finish. What can I coat it with first that will allow me to sand and then do the final powder coat?