hey all. i need some advice.there seams to be a fine line between curing time and temp when it comes to this powder.
temp that rises too fast seams to create more orange peal.like the powder cures before it has the chance to fully flow out.also the metal pigment sometimes wont rise fastenough and leaves black pockets .like some kind of contamination.
also film thickness is very sensitive.if it is too thick and the temp rises too fast it flows out and seams to seperate so there are these streaks in it.
has anyone had similar problems?any tips?