Alright, I just did a customers alluminum swingarm tonight, I was very very careful and clean. I outgassed it for 25min at about 390-400. Hotflocked it at about 170 deg. then baked for 10 min after flowout.
MASSIVE OUTGASSING!!! PINHOLES EVERYWHERE CRAP!! 😡 😡
Do I have to strip it back down or can I throw another coat over it tomorrow or does that not work??