Fillers for PC

Viewing 1 post (of 1 total)
  • Author
    Posts
  • #31516

    i know this has been discussed here and there, and even after more searching i didn’t find good answers. i have a project that will require filling, and two coats of powder. so i seem to be limited to the hi-temp lab metal for multiple bake cycles?

    for pieces that require a skim coat, it sounds like all metal is best?

    also, has anyone tried the thermobond3?