    Alumablast quart purchased mixed well then shot in 90 degree weather yet its been 9 days. Still the paint is very very soft and tacky. Some of the parts I could remove paint and reshoot if I had to but it was shot on the sides of a powder coated gas tank. Reshooting that will prove to be very difficult. Anyone else have this issue?